采用搅拌法制备了Al-2.15%Mn合金
对其显微组织、强化机制及摩擦磨损性能进行了试验研究.结果表明:Al-2.15%Mn合金的组织为含Al
11
Mn
4
和Al
6
Mn的α-Al固溶体; 合金中Al
6
Mn的沉淀强化作用使其硬度较纯Al提高了60%; 纯Al的冲击断口形貌为塑性断裂
Al-2.15%Mn合金的冲击断口形貌为准解理断裂; 纯Al与Al-2.15%Mn合金在湿摩擦下的磨损量均大于干摩擦的磨损量; 湿摩擦的腐蚀-机械磨损作用使磨痕为犁沟和蚀坑
干摩擦中磨屑的成片脱落由机械磨损中的黏着磨损引起; 在干摩擦与湿摩擦中
纯Al的摩擦因数均大于Al-2.15%Mn合金的摩擦因数
Al-2.15%Mn合金较纯Al表现出更加优良的耐磨性.
Al-2.15%Mn alloy was fabricated by stirring casting. Its microstructure
strengthening mechanism
and friction and wear behavior were investigated. The results show that: 1)The as-cast microstructure of Al-2.15%Mn alloy is composed of α-Al matrix with Al
11
Mn
4
and Al
6
Mn compounds; 2)The hardness of Al-2.15%Mn alloy gets 60% higher than that of pure aluminum because of deposition strengthening by Al
6
Mn; 3)The impact fractures exhibit plastic morphology for pure aluminum and quasi-cleavage morphology for Al-2.15%Mn; 4)The worn mass losses of both pure aluminum and Al-2.15%Mn alloy under lubricating condition are greater than that under dry condition because combination of corrosion and mechanical wear in wet friction condition generates furrows and corroded pits on sample surface
while adhesive
wear in dry friction condition makes worn chips flake off the sample surface; 5)Al-2.15%Mn alloy shows smaller friction coefficient and better wear resistance than pure aluminum in both wet and dry wears.
SHARMA M M. Microstructural and mechanical characterization of various modified 7XXX series spray formed alloys [J].Materials Characterization, 2008, 59(1): 91-99.
SHARMA M M, AMATEAU M F, EDEN T J. Mesoscopic structure control of spray formed high strength Al-Zn-Mg-Cu alloys [J]. Acta Materialia, 2005, 53(10): 2919-2924.
SHIMIZU H, OSAMURA K, ADACHI H, et al. Influence of additional Mn and Cu contents on mechanical properties of Al-Zn-Mg ternary based alloys [J]. Journal of Japan Institute of Light Metals, 2004, 54(1): 2-8.
FILATOV Y A, YELAGIN V I, ZAKHAROV V V.New Al-Mg-Sc alloys [J].Materials Science and Engineering: A, 2000, A280: 97-101.
BEREZINA A L, CHUISTOV K V, KOLOBNEV N I, et al. Sc in aluminum alloys [J].Materials Science Forum, 2002, 396/397/398/399/400/401/402: 74l-746.
PARKER B A, ZHOU Z F, NOLLEX P. The effect of small additions of scandium on the properties of aluminum alloys [J]. Journal of Materials Science, 1995, 30(9): 452-458.
HAYNES M J, GANGLOFF R P. Elevated temperature fracture toughness of A1-Cu-Mg-Ag sheet: characterization and modeling [J].Metal Trans: A, 1997, A28(9):1815-1829.
XIAO Daihong, WANG Jiannong, DING Dongyan. Effect of Cu content on the mechanical properties of an Al-Cu-Mg-Ag alloy [J].Journal of Alloys and Compounds, 2002, 343(1/2): 77-81.
肖代红,王健农,陈世朴,等.微量Ag对A1-5.3Cu-0.8Mg合金组织和耐热性能的影响[J].机械工程材料, 2003, 27(1): 38-40.
XIAO Dai-hong,WANG Jian-nong,CHEN Shi-pu,et al. Effect of small amount of Ag on microstructure and mechanical properties of an A1-5.3Cu-0.8Mg alloy [J].Materials for Mechanical Engineering, 2003, 27(1): 38-40.
倪红军,孙宝德,蒋海燕,等.稀土熔剂对A356合金二次枝晶臂间距的影响[J].中国有色金属学报, 2002, 12(5): 940-944.
NI Hong-jun,SUN Bao-de,JIANG Hai-yan,et al. Effect of rare earth flux on secondary dendrite arm spacing of A356 alloy [J]. The Chinese Journal of Nonferrous Metals, 2002, 12(5): 940-944.
WANG S C, ZHU Z, STARINK M J. Estimation of dislocation densities in cold rolled Al-Mg-Cu-Mn alloys by combination of yield strength data, EBSD and strength models [J]. Journal of Microscopy, 2005, 217(2): 1-5.
耿兴国,傅恒志.Al-Mn合金快速定向凝固组织中的带状结构[J].西北工业大学学报, 2004, 22(2): 247-250.
GEN Xingguo, FU Hengzhi. Determination of difficult-to-determine banding structure during high rate directional solidification of Al-Mn alloy [J]. Journal of Northwestern Polytechnical University, 2004, 22(2): 247-250.
樊自立,王喜鹏. 新疆平原湖泊(包括人工湖)水质盐化及其防治途径[J].自然资源学报, 1990, 5(4): 311-314.
FAN Zi-li, WANG Xi-peng. Water salinization of plain lakes(including man-made lakes)and its prevention and control in Xinjiang [J]. Journal of Natural Resource, 1990, 5(4): 311-314.
林肇琦.有色金属材料学[M].沈阳:东北工学院出版社, 1986: 1-51.
上海市机械制造工艺研究所.金相分析技术[M].上海:上海科学技术文献出版社, 1987: 742-743.
CARROL M C. Improvements to the strength and corrosion resistance of Al-Mg-Mn alloys of near-AA5083 chemistry [D]. Kolumb, USA: The Ohio State University, 2001.
石敏,刘炳,孙金梅.锰含量对铝锰合金冲击韧度和金相组织的影响[J].热加工工艺, 2010, 39(18): 13-19.
SHI Min, LIU Bing, SUN Jinmei. Effect of Mn content on impact toughness and metallurgical microstructure of Al-Mn alloy [J]. Material Heat Treatment, 2010, 39(18): 13-19.
柳伟,郑玉贵,姚治铭,等.CrMnN不锈钢的抗空蚀和磨蚀性能[J].材料研究学报, 2001, 15(5): 505-509.
LIU Wei, ZHENG Yu-gui, YAO Zhi-ming, et al. Resistance to cavitation erosion and cavitation-abrasion of CrMnN stainless steel [J]. Chinese Journal of Materials Research, 2001, 15(5): 505-509.
彭成章,朱玲玲.电沉积Ni-P/纳米Al2O3复合镀层的摩擦磨损与耐铝液侵蚀性能[J].中国有色金属学报, 2010, 20(6): 1177-1182.
PENG Cheng-zhang, ZHU Ling-ling. Tribological properties and erosion resistance of electroplated Ni-P/nano-Al2O3 composite coatings to aluminum liquid [J]. The Chinese Journal of Nonferrous Metals, 2010, 20(6): 1177-1182.
李新梅,刘炳,董晓锋. Al2O3颗粒增强Al-Mn合金基复合材料的制备及摩擦学性能[J].材料热处理学报, 2011, 32(7): 6-11.
LI Xin-mei, LIU Bing, DONG Xiao-feng. Fabrication and friction and wear behavior of Al2O3 particulates reinforced Al-Mn alloy matrix composites [J]. Transactions of Materials and Heat Treatment, 2011, 32(7): 6-11.
WILSON S, ALPAS A T. Wear mechanism map for meal matrix composites [J]. Wear, 1997, 212(4): 41-49.
0
浏览量
4
下载量
2
CSCD
关联资源
相关文章
相关作者
相关机构
京公网安备11010802024621